Dec 8, 2008

CSB to Conduct Full Investigation of Causes of Catastrophic Fertilizer Tank Collapse at Allied Terminals in Chesapeake, Virginia; Issues Urgent Safety Recommendations Citing Hazard to Public from Welding Defects on Several Remaining Tanks